The chart below shows a sharpness comparison between the AutoEdge and two competitors' edges. This test, conducted in accordance with ISO standard 8442-5.2004, simulates heavy production usage by repetitively pushing the edge through abrasive-coated card stock and measuring the depth of each successive cut.
The AutoEdge delivers initial sharpness as much as 76% higher than its competitors, as seen at the left of the chart, and even at 60 test cycles, gives cutting performance 4x that of the other edges.